AM50A 12kg

Standard Magnesium Alloy

Typical Application: Die Casting

Configuration: Alloy

AM50A 12kg
Chemical Composition: ASTM B93/B93M Composition in % (Max) | AM50A Mg Remainder Al 4.5-5.3 Mn 0.28-0.50 Be 0.0005-0.0015 Zn 0.2 Si 0.05 Cu 0.008 Ni 0.001 Fe 0.004 Other elements each 0.01 Mechanical Properties: Properties | AM50A Tensile yield strength [MPa]20°C 120 Ultimate tensile strength [MPa] 20°C 150°C 260 130 Compression yield strength [MPa] 125 Elongation in 50 mm [%] 19 Impact strength [J](2) 22 Young's Modulus [GPa] 45 Hardness, Brinell 60 Fatigue strength [MPa](3) 90 Creep strength:Stress to produce 0.2% strain in 100 hr at 150°C [MPa] - Physical Properties: Typical Physical Properties Properties | AM50A Density at 20°C [g/cm3] 1.77 Lin.thermal exp.Coeff [μm/m.K] at 20-100°c 26.0 Thermal conductivity [W/K m] at 20'C 65 Electrical conductivity at 20'C[W/K.m) 9.1 Specific heat [kJ/kg K] at 20'C 1.02 latent heat of fusion [kJ/kg] 370 Non-equilibrium Solidification range[°c] 620-434 Ingot Dimensions: Weight Length Width Height kg | Lb mm | inch mm | inch mm | inch 12 | 26.4 627 | 24.7 130 | 5.1 89 | 3.5 Typical bundle dimensions: ingots: 54 Layers: 11 Weight Length Width Height kg | Lb mm | inch mm | inch mm | inch 648 | 1428 627 | 24.6 627 | 24.6 979 | 38.5 Wooden Pallet    

Green Pallet